BS EN ISO 15614-2:2005 – Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 2: Arc welding of aluminium and its alloys

BS EN ISO 15614-2

1 Scope
This document specifies how a preliminary welding procedure specification is qualified by welding procedure tests.
This document is part of a series of standards, details of this series are given in EN ISO 1 5607:2003, Annex A.
This document defines the conditions for the execution of welding procedure tests and the range of qualification for welding procedures for all practical welding operations within the range of variables listed in Clause 8.
This document applies to the arc welding of wrought and cast aluminium and its alloys. In this document the term aluminium stands for aluminium and for aluminium alloys.
This document does not apply to finishing welding of aluminium castings which is dealt by prEN ISO 1 561 4-4.
Arc welding of aluminium is covered by the following welding processes in accordance with EN ISO 4063:1 31 : metal inert gas welding (MlG welding);
1 41 : tungsten inert gas welding (TlG welding);
1 5 : plasma arc welding.
NOTE Specific service, material or manufacturing conditions may require more comprehensive testing than is specified by this document (see 7.1 ).
The principles of this document may be applied to other fusion welding processes.
2 Normative references
The following referenced documents are indispensable for the application of this document. For dated eferences, only the edition cited applies. For undated references, the latest edition of the referenced document (including any amendments) applies.
EN 51 5, Aluminium and aluminium alloys — Wrought products — Temper designations.
EN 571 -1 , Non destructive testing — Penetrant testing — Part 1: General principles.
EN 1 71 4, Non-destructive examination of welds — Ultrasonic examination of welded joints.
EN ISO 6947, Welds — Working positions — Definitions of angles of slope and rotation (ISO 6947:1993).
EN ISO 9606-2, Qualification test of welders — Fusion welding — Part 2: Aluminium and aluminium alloys (ISO 9606-2:2004).
EN ISO 1 5607:2003, Specification and qualification of welding procedures for metallic materials — General rules (ISO 15607:2003).
EN ISO 1 5609-1 , Specification and qualification of welding procedures for metallic materials — Welding procedure specification — Part 1: Arc welding (ISO 15609-1:2004).
EN ISO 1 561 3, Specification and qualification of welding procedures for metallic materials — Qualification based on pre-production welding test (ISO 15613:2004).
ISO 41 36, Destructive tests on welds in metallic materials — Transverse tensile test.
ISO 51 73, Destructive tests on welds in metallic materials — Bend tests.